Kamil, M. P., Puranto, P., Suwondo, K. P., Wong, L. M., Zhang, Z., Seng, D. H. L., Kozin, M., & Wang, S. J. (2026). pH-dependent corrosion behaviour of Al alloy: comparative roles of native and surface-applied Al2O3 layers. Surfaces and Interfaces, 97, 110223. https://doi.org/10.1016/j.surfin.2026.110223
Abstract:
Aluminium (Al) alloys are widely used in strategic applications that benefit from lightweight structures, but they remain highly susceptible to corrosion in aggressive pH conditions. In this work, the corrosion behaviour of Al alloys with natural or artificial Al2O3 surface layers was investigated in NaCl 3.5 wt.% solution adjusted to pH 2, pH 7, and pH 12. Polarization tests showed that the dense ∼200 nm sputtered Al₂O₃ layer provided the highest protection efficiency (PE) value of 96.63% in neutral solution, whereas the thicker ∼5 µm plasma electrolytic oxidation (PEO) coating was more effective under aggressive pH conditions despite its open porosity, achieving PE values of 94.78% in pH 2 and 99.65% in pH 12. Electrochemical noise analysis revealed that corrosion responses in pH 12 caused the most unstable oscillations in uncoated and sputter coated specimens: low Rn, high ΨI, and steep PSD slopes approaching 1/f² behaviour, indicating repeated film breakdown and repassivation. On the other hand, PEO-coated specimen exhibited a quasi-steady current response in pH 12, suggesting sustained oxidation/dissolution rather than intermittent burst-dominated corrosion. Time-dependent impedance measurements up to 24 h confirmed the strong pH dependence responses, where pH 2 and pH 7 generally caused impedance degradation due to oxide/passive-layer dissolution, whereas pH 12 induced an unusual progressive impedance increase associated with the formation of corrosion-derived barrier layers. Post-corrosion analyses corroborated the electrochemical interpretations by linking the pH-dependent responses to distinct surface damage modes, corrosion-product accumulation, and oxide/hydroxide/chloride participations
License type:
Attribution-NonCommercial-NoDerivatives 4.0 International (CC BY-NC-ND 4.0)
Funding Info:
This work was supported by the Research Organization for Nanotechnology and Materials – National Research and Innovation Agency (BRIN), Republic of Indonesia, through research grants under contract numbers 2/III.10/HK/2025. This research is also supported by Singapore Academies Southeast Asia Fellowship (SASEAF - SC49/24–700200), in conjunction with Future Energy Acceleration & Translation (FEAT) Programme, A*STAR.